TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Date:
Mon, 26 Nov 2001 14:11:57 -0600
Content-type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
The issue of long term storage of parts or boards is not a new one.   The
military, faced with REALLY long lifetimes (e.g. 50 years for a MX missile)
and decreaseing market clout, has had to deal with lifetime buys for a long
time.  In my mind, there are two possibilities:  (1) preserve the original
solderability for as long as possible, or (2) plan on restoring the
solderability at some point in the future when the part is needed.

In the first case, you will have to setup some fairly elaborate storage
conditions where oxygen and moisture are excluded.  Dry nitrogen is most
common, but alternatives could include dessicated conditions or coverage
with a heavy noble gas like argon.  You will have to setup incoming and
outgoing logs that tightly control the inventory, and you have to have
floor space for the storage for the life span of the part.

In the second case, you restore the solderable surface.  Some people do
this using aggressive fluxes and re-tinning, with limited success.  An
alternative to this is to use an electrochemical reduction process called
ROSA to change the surface oxides to the base metal, restoring
solderability.  ROSA can be done on many parts at the same time, it is
electroless, and is not too capital intensive.  Dave Hillman of Rockwell is
the master of ROSA and has published a number of papers on the topic.  He
would probably answer more fully but he is currently putting the finishing
touches on his Master's thesis and so won't stick his head out of his
cubicle for another few days.  And when he does, if he sees his shadow,
there will be 5 more months of winter (in Iowa, that's a safe bet).  Where
was I?

The advantage of the ROSA approach is that it does not matter all that much
what the solderability condition was when the part was received, and the
storage conditions do not have to be draconian.

As the commercial goes, you can pay me now or pay me later.....

Doug Pauls
Rockwell Collins

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2