I think he means 2.5 deg C/min which is about 4.5 deg F /min, which is still quite slow. 10-12 might be higher than optimum as well. Many products recommend 8-12 degF/min or so.
5 deg C/min (9 deg F/min) is probably safe for just about any FR-4 type product.
As far as the KISS cycle goes, usually you want to increase to high pressure at about 200-220F. Earlier is better than later.
Best Regards,
Timothy Reeves
Technical Service Engineer - Matsushita Electronic Materials, Inc.
4114 Heather Street, Forest Grove, Oregon, 97116
Main (503) 357-8695 Direct (503) 992-5109 Cell (503) 781-1495 Fax (503) 357-8868
-----Original Message-----
From: Rick [mailto:[log in to unmask]]
Sent: Tuesday, March 25, 2003 4:14 AM
Subject: Re: Laminate voids & resin recession
2.5 deg/min. is a little slow. Try and aim for 10-12 deg/min. The
lower the rate of rise the more viscous the resin which means it
won't flow as much. Also, try going into full pressure right away.
This will also force the resin to flow. I've found kiss cycles don't
buy you much plus the operator might forget to go into full pressure
before the resin starts to cure (if you're press doesn't do it
automatically). Double check your vacuum pressure. You should
have at least 27 in. Hg.
Rick Babyak
Process Engineer
Proto Circuit Inc.
7 Ascot Parkway
Cuyahoga Falls, OH 44223
330-572-3400
330-572-3434 fax
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|