In a message dated 09/22/1999 12:24:13 PM Central Daylight Time,
[log in to unmask] writes:
<< Technetters
I have a situation where I need the advice from the Technetters. I have an
assembly with HASL. In order to stay within the aspect ratio guidelines, I
must use a stencil that has a .0085 aperature opening, a 20 mil spacing, and
I must use a 6 mil stencil. I tried this and when the stencil pulled away,
the surface tension pulled away the solder paste from the pad area. If I
were to go to a 5 mil stencil (which is outside the Aspect Ratio
guidelines), would this help me with keeping the solder paste on the pad and
not on the stencil? Or is there another approach that I should consider
instead of going to another stencil thickness? Any help you can give me
would be appreciated
Donn E Steffen
Senior Quality Engineer
VDO Control Systems
Auburn, IN 46706
Phone (219)925-8887
Fax (219)925-8710
Email: [log in to unmask] >>
Hi Donn!
The aspect ratio I've always went by was that the aperture width needed to be
1.5 times the stencil thickness, so in a 6-mil thick stencil the minimum
opening would need to be at least 9-mils wide (with nice sidewalls) But even
9-mils is pushing it. The minimum width that I always use is 10-mils wide for
a 6-mil stencil to avoid the problem you're having. If I go less than 10,
I'll start reducing the thickness of the stencil. Separation speed also plays
a big part whether the paste hangs up in the stencil from my
experience...it's like if you separate the foil from the board n-i-c-e and
s-l-o-w after the print stroke, the paste will ease out of the apertures and
give you a nice solder brick on the pad...
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|