Ladies and Gentlemen,
my company is evaluating conveyorized solder stripping equipment/chemistry
and I'm facing a problem. Our water treatment system is a selective IX
system and the resin that we are using to extract lead requires a pH
adjustment to approx 4 pH to be effective. Now, the problem is that at
about 3 pH the iron that is in most nitric based solder stripping
chemistries precipitates creating a huge mess.
The chemistry that we are using now (in a vertical batch system) is iron
free but I am told that a horizontal conveyorized system needs a ferric
chemistry to be effective.
Two questions:
1. is there a chemistry that is iron free AND will perform well in a
horizontal setup?
2. is there a lead treating resin for ion exchange water treatment that
works well at approximately 2.5 pH?
Any help will be greatly appreciated
Kiko Vigano
------------------------------------------------------------------------
Adeodato Vigano
Production Manager
Compunetics, Inc. - PCB Division
(412) 858-6115
[log in to unmask]
------------------------------------------------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|