Zinc plate may show a lite brown depending on the bath.   Passivation is a
acid bath
to remove machining oils etc.  No rust preventation properties.

----- Original Message -----
From: Ken Patel <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 25, 2002 1:43 PM
Subject: [TN] Sheet Metal Plating


> Hello there,
> We are seeing some sheet metals with problems like corrosion, finger
> print and some kind of weird brown spot on them. we have specified
> Bright Zinc Plating on them. I am interested in sending this to any
> local lab fro analysis.
> (1) Name of any lab where I send them for analysis, preferably local in
> San Jose Bay Area.
> (2) Should I change the plating spec?
> (3) What is passivation?
>
> My vendor was suggesting Double Zinc Plating. Any help will be highly
> appreciated.
>
> Re,
> Ken Patel
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2