TECHNET Archives

December 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Thu, 4 Dec 2008 13:15:49 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (98 lines)
Well, take a stab at it, but only if you have a good point.....

Doug Pauls
Rockwell Collins



John Burke <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
12/04/2008 11:37 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
John Burke <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] NTC [TN] Materials






So does a handwritten note on a slash sheet constitute a cutting remark?

John Burke
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey 
(EHCOE)
Sent: Thursday, December 04, 2008 9:05 AM
To: [log in to unmask]
Subject: [TN] Materials

To all,

We are working these issues. There are upgrades needed on the slash
sheets. Some of the test methods are archaic and need replaced or at
least up-graded. The minimum limits in some cases need to be raised and
the playing field narrowed. A new thermal stress test  is being
developed to simulate lead-free processing conditions as well as a new
delam coupon, which will hopefully better predict usability/reliability
of a chosen slash sheet laminate material. The STII and other material
requirements need to be first incorporated in IPC-2221 and IPC-6012 to
allow a designer to choose based on needed material performance versus
design knowing the processing parameters involved as well as the end use
environment.

Please join us in this effort by coming to the meetings and lending your
support and technical input. I'll handle the humor.

Dewey


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2