TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 7 Dec 2005 15:23:39 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (90 lines)
Hi Vicka! Here are the numbers my references have:

For Acid copper         1.70-1.82 microohm-cm
For Pyrophosphate copper      1.73-1.75 microohm-cm

The specific bath chemistry and additives seem to push the resistivity
values around.

Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             "White, Vicka
             (AZ75)"
             <vicka.white@HONE                                          To
             YWELL.COM>                [log in to unmask]
             Sent by: TechNet                                           cc
             <[log in to unmask]>
                                                                   Subject
                                       [TN] Resistivity of plated copper
             12/07/2005 02:59
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               "White, Vicka
                  (AZ75)"
             <vicka.white@HONE
                YWELL.COM>






Does anyone have accurate information of the resistivity of plated
copper as compared to copper foil?
I have done some research and found that there are a lot of conflicting
statements out there. I have seen it published anywhere from plated
copper being 4.8 to 6 uohm cm.



Vicka White
PWB Technology
Honeywell - Phoenix

Email: [log in to unmask]
Phone: 602-436-1467
FAX: 602-436-2252
Pager: 602-238-8274





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2