     Oops.. forget the decimal point it is less than 15 microns.


______________________________ Reply Separator _________________________________
Subject: Re: Drilling spindle runout
Author:  "LIM BOON HOCK" <[log in to unmask]> at INTERNET
Date:    09/26/96 6:49 


Are you really able to achieve 1.5 micron dynamic runout ? Are yours  new 
drilling machines? I am asking this because some info I have from two 
companies said they are controlling at 10 and 15 micron (dynamic runout) 
respectively. Maybe you can share some tips on how you can manage to 
achieve such a low runout. I would appreciate that. 
     
To other technet users in the drilling section, is 1.5 micron dynamic 
runout the norm in your control of dynamic runout?
     
Regards
     
----------
> From: [log in to unmask]
> To: [log in to unmask]
> Subject: Re: Drilling spindle runout
> Date: Wednesday, September 25, 1996 1:05 AM 
> 
>      We are controlling to less than 1.5 microns, dynamically at 80K rpm. 
> 
> 
> ______________________________ Reply Separator 
_________________________________
> Subject: Drilling spindle runout
> Author:  [log in to unmask] at INTERNET 
> Date:    09/24/96 9:23 
> 
> 
> I would like to know for the drilling machines used in the manufacturing 
of 
> pcb's, what is the dynamic runout (in micron) that you(for those involve)
     
> are controlling. Replies are very much appreciated. Thanks 
>      
> Regards
>      
>
***************************************************************************
     
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 
* 
>
***************************************************************************
     
> * To unsubscribe from this list at any time, send a message to:          
* 
> * [log in to unmask] with <subject: unsubscribe> and no text.       
* 
>
*************************************************************************** 
>      
>      
> 
>
*************************************************************************** 
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 
*
>
*************************************************************************** 
> * To unsubscribe from this list at any time, send a message to:          
*
> * [log in to unmask] with <subject: unsubscribe> and no text.       
*
>
*************************************************************************** 
> 
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2