TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
David Taylor <[log in to unmask]>
Date:
Thu, 11 Sep 1997 09:19:32 +1000
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, David Taylor <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
Hello Technetters,

We are looking for some feedback on what types of finishes other PCB
manufacturers are using on SIMM and DIMM modules.

Solder levelled with hard gold/nickel edge contacts.

OSP with hard gold/nickel edge contacts.

Hard nickel/gold flash all over. 2.5um Ni over 0.75um Au

Electroless nickel/gold.

etc etc etc.


Regards,

David Taylor
Chief Engineer
East Coast Printed Circuits
61 2 9982 1377 Ph
61 2 9971 0437 Fax

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2