Pradeep , If you are having difficulty locating the shorts using
Richard's suggestion, I might be able to help. If you can send me a
board (postpaid, both ways), I have a non-contact probing method to
locate the position of the short.
Later,
Carl Van Wormer, P.E., AE7GD
www.testecvw.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, March 29, 2012 5:16 AM
To: [log in to unmask]
Subject: Re: [TN] Short after assembly
Same inputs as before. We can't find the short for you. Time to get out
the precision ohmmeter and start probing.
Lay down a sheet of white shelving paper. Pick up the assembly, turn it
over, and shake vigorously over the paper. See what falls out. Then
re-test.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pradeep Menon
Sent: Thursday, March 29, 2012 6:49 AM
To: [log in to unmask]
Subject: [TN] Short after assembly
Importance: High
Dear all,
Thanks for the inputs on my last query. In the meanwhile we have got
some more details on the same issue which we would like to share.
This is a 6 layer board manufactured with Nelco 4000-6 (Tg175deg)
material with laminate construction. We had fabricated this board 2-3
years back. We had done the isolation test in our BBT at 10Mohm
threshold. The board was assembled and was working perfectly.
The customer does a continuity and isolation test after assembly. Then
they have done a thermal cycling for the package in powered OFF
condition. Ie 3 cycles at 13 deg C and 60 deg C with 45 minutes duration
at both temperatures. Then with the powered ON condition 2 cycles at 13
degC and 60deg C with 45 minutes duration at both temperatures.
Functional check and performance was confirmed after that. This is the
standard procedure.
But for this package, they have carried out an additional thermal
cycling over and above the normal thermal cycling procedure indicated
above. This time they have done a thermal cycling for the package in
powered OFF condition. Ie 3 cycles at 13 deg C and 60 deg C now with 100
minutes duration at both temperatures. Then with the powered ON
condition 2 cycles at 13 degC and 60deg C with 45 minutes duration at
both temperatures. Functional check and performance was verified and
this time they found a short between 2 points. And this is not a low
resistance short as per the customer, it is a 0ohm dead short.
Now we have been asked to analyse the same. Can you pls give some inputs
for this
Rgds
Pradeep
From: Pradeep Menon
Sent: Tuesday, March 27, 2012 5:03 PM
To: [log in to unmask]
Subject: Short after assembly
We had supplied a PCb to one of our high reliability customers 2-3 years
back. Now we understand that in one of the PCB they have observed a low
resistance short after thermal cycling. The bare PCB was BBT tested at
our end and was also cross verified as a bare board by the customer.
They had populated the board and the tests were all found compliant.
After some time they say they observed a low resistance short. We are a
bit perplexed on this. Can anyone share what can be the possible reasons
for the same. We feel it may be even something to do with assembly as
well. Can you pls provide some inputs
Rgds
Pradeep
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|