Our company for Military contracts used to perform a high humidity mealing
test monthly. This
would show that the process was acceptable. Silicone MFP was more sensitive
to soils and mealing
than Urethane.
-----Original Message-----
From: Kenny Bloomquist [mailto:[log in to unmask]]
Sent: Friday, November 19, 1999 9:54 AM
To: [log in to unmask]
Subject: [TN] Speaking of Adhesion of Conformal Coating
I'm curious what other companies do as an in process test for conformal
coat adhesion, if anything.
I'm particularly interested in Parylene but also curious about UR and AR.
If you do in process testing what spec do you follow, if any, and what
materials do you use, i.e. tape type, Exacto, etc.
Thanks to all responders,
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|