In a message dated 9/14/06 8:59:59, [log in to unmask] writes:
> Werner,
> I understand your point, but the temp stress really is relative to
> the product being tested and the purpose of the testing. In one case I
> perform infant motality screen at -10C to +70C while the product runs
> through functional testing. There are other stresses applied at the
> same time....voltage...frequency...etc... It really is impossible to
> give a blanket statement that a specific temp stress is good for all
> applications. There are a lot of variables that need to be considered
> in each case. A better question for a newcomer may be.....What
> variables should I consider and what is the formula to determine the
> proper stress temp. It's not an easy process.
>
Hi Barrie,
I fully agree. That is why I am giving workshops on this subject matter.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|