Hello,
I have a PCA that hand solders 6 connector pins to an 4 layer PCB
assembly.
The finish on the PCB is Lead Free HASL (SN100CL) and the solder used to
hand solder the pins is SAC305. The hand soldering is performed as a
secondary assembly operation after reflow.
What happens to some of the assemblies, but not all of them, is that the
solder will wick straight up the pin, thereby not allowing a Solder joint.
The pin can be pulled right out of the hole, revealing a PTH with no
inner barrel.
Completely wiped out as if it was never there in the first place. This
phenomenon is not present on every PCB or every pin of the same connector.
The PCB's are part of a multi-board panel.
As far as I know the PCB started out with a barrel, but I cannot rely on
this being the case as I do not believe the technician checks 100% of the
PTH's prior to inserting the pin.
Am I looking at excessive heat causing complete Copper Dissolution of the
PTH barrel?
or
A PCB that may not have a barrel in every hole, part of the PCB
fabrication process?
or
Any other suggestion as to which direction to head would be appreciated.
Thanks in advance.
Tom Burek, CID+
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|