TECHNET Archives

December 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 12 Dec 2013 08:37:24 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
Parts/Attachments:
text/plain (7 lines)
In the past, we specified starting foil thickness and finished thickness.  It was a legacy thing, no one knows where it came from.  Realizing that copper is copper, and the vendor knows their process requirements, we recently removed the foil requirement and specify only minimum or nominal finished copper thickness.  Save s a lot of emails.


And I agree with Grunde, the IPC document charts are informative beyond just specifying a requirement.  Maybe they could be reworked to be more clear, but keep the additional data.

Pete