Louis,
Your customer specification ought to tell you whether a coating is required
or not. Generally they do.
You state that the circuit is small and there is a lot of masking (and
therefore de-masking) involved before spraying. How about brushing the
coating?
As an alternative, you could try using a small dispenser such as EFD with
the syringe pre-loaded with the coating material.
Furthermore, I would expect that the coating has to qualified to the US
MIL-I-46058. If so, these must contain a UV tracer to aid inspection. So, if
you do this coating work under a black (UV) light source, then you can see
very clearly where you are putting it - and where you shouldn't!!
Hope this helps,
Regards, Graham Naisbitt
[log in to unmask]
Concoat Ltd Phone: +44 1276 691100
Alasan House Fax: +44 1276 691227
Albany Park
CAMBERLEY
GU15 2PL UK
Any opinions expressed are those of this employer.
-----Original Message-----
From: Louis, Edwin <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 02 February 1999 17:58
Subject: [TN] Conformal Coating on Naval Avionics PWAs
> Is there anyone out there who knows if conformal coating is necessary
> for Naval Avionics Printed Circuit Assemblies? We are having problems
> applying coating to small PWAs with gold areas on the boards.THe cost
> of doing intricate masking before spraying is very high.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|