TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Thu, 3 May 2007 21:03:33 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Werner, pic 1 and 2, what I call good joints, are several times stronger 
than ther "rotten" ones. These later crack , and the leads separate from the 
pad clearly. Lifted is too strong a word, but they are disconnected by as 
much as one third the lead thickness. My customer has spent months to find 
out why.
Inge


----- Original Message ----- 
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 04, 2007 12:34 PM
Subject: Re: [TN] Metalurgists, need assistance


Hi Ingemar,
Looking at pic1, I would not call what I am seeing a "good joint"—it is an
interfacial separation, and thus the interface [whatever it is] is the weak. 
and
unpredictable, link.
Pic3 looks more like a ductile separation—see the directionality of the
cup-like 'voids', in the solder [easy to confirm if the composition is the 
same on
both fracture surfaces.] Pic4 looks like the Ni layer is showing 
through—>the
solder properly wetted in some areas, but not all.
Sn spheres—beats me.



Werner



**************************************
 See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2