TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Bill Fabry <[log in to unmask]>
Date:
Tue, 23 Jun 1998 14:45:28 -0700
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (27 lines)
Techies:

Thanks for your response to the above-mentioned topic.

As it turned out, the root cause of the problem wasn't as difficult or
"off-the-wall" as I originally thought it to be.  Steve Gregory hit the nail on
the head.

Our assembly subcontractor splashed solder on the adjacent gold fingers during
component replacement.  They used in-house gold replating operation to resurface
the fingers and were a bit overzealous in the plating, causing the MELF
terminals to be inadvartantly coated along with the fingers with the "new" gold.

Bill Fabry

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2