TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Sun, 15 Aug 2010 20:55:45 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (136 lines)
"The absolute last thing they should be doing is asking an assembly house to
specify a potting material in an RF design and then ask the vendor of the
material if it is going to be an issue...."
May be they should fork over part of designer's salary as well?  When the design give away the selection of the materials, it smells big trouble.  Run, like hell. .

--------------------------
Sent using BlackBerry


----- Original Message -----
From: John Burke [mailto:[log in to unmask]]
Sent: Sunday, August 15, 2010 06:13 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Is Calcined alumina in Epoxy resist tramission signal..?

Hi hetal,

Maybe they should be asking why they are potting at all? (maybe a conformal
coating with parylene?)

Honestly from your mail the design team seem to be disconnected with
reality.

Used to be that they would take the RF properties of their proposed design
into account and arrange materials/ RF power output (for
transmission)/front end amplification (for receivers) into account.

The absolute last thing they should be doing is asking an assembly house to
specify a potting material in an RF design and then ask the vendor of the
material if it is going to be an issue.....

Suggest that the assembly house might want to push back on this and ask what
exactly the attenuation limits of the materials should be in order for the
design to pass DVT/PVT testing.

On the mechanical issue I have seen assemblies use a 2 part potting process,
the first as a semi-compliant coating, the second as an epoxy coating over
the top of the first.

I am sure others here on TechNet will be able to help on the mechanical
questions.

On the RF performance the designer will need data sheets on the materials
and a mechanical estimation of the depth of potting materials over the
board/transmission component surfaces - he will need data on dielectric
constant of the materials - and to be honest to avoid problems of the
assembly house facing "failed on test yield" issues I would recommend a full
pilot run with DVT and PVT testing on the pilot units. Unless they have a
master plan for re-working potted assemblies?...............8-)

Best regards,

John Burke

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hetal Shah
Sent: Thursday, August 12, 2010 10:08 AM
To: [log in to unmask]
Subject: [TN] Is Calcined alumina in Epoxy resist tramission signal..?

Our customer  have an RF Transmitter on the PCB. they have a couple of
concerns.
 One that the potting material will damage the components and the other that
the potting material will shield the RF Transmissions of their transmitter.

Their assembly house was going to use our 2 parts Epoxy (which conatains
Calcined alumina) as the potting material.  Will this create any of the
problems mentioned?


Any insight into this matter would greatly be appreciated.



Thank you

Hetal Shah

R & D Chemist

MG Chemicals


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2