TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Sauer, Steven T." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 22 Jan 2004 07:26:55 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (50 lines)
Good Morning Steve,
Several things that I've seen which "requires" dry film are:
1) Legacy drawings for circuit cards designed in the 80's that we still
produce, and
2) New drawings when the draftsperson or layout designer has cut and pasted
notes from old legacy drawings noted in 1 above.

I attempt to review every drawing before it is released and getting "B2"
changed to "B1" before the fabricator gets it.  The other wicket is our
suppliers request relief from the dryfilm and provide LPI, which requires a
modification to the PO.  We own the majority of our data packages, therefore
customer consent is typically not required.

IMHO with the advancements in material technology and photoimaging
equipment, the person who selects dryfilm doesn't understand the big
picture.  A side by side comparison with pros and cons should shed an
immaculate light.  Let's face it, solder mask was designed as a process aid
to minimize solder bridging during mass soldering (i.e. wave, drag & vapor
phase) processes and was never intended to be relied upon as a dielectric
nor insulator.  A lot of the "old school" information is continually being
lost and that is directly proportional to the amount of "how to" being
removed from specifications and standards.  As you can tell I'm not a fan,
nor ever will be of the DOD Standardization Reform but I do know that a
solder connection doesn't have to bright and shiny to be reliable!!
Good Luck!

Steve Sauer
Sr. Mfg Engineer
Northrop Grumman, Electronic Systems
Xetron

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, January 21, 2004 8:17 PM
To: [log in to unmask]
Subject: [TN] Why Dry film Solder Masks?


Can anybody tell me why dry film solder masks are still specified?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2