TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sun, 31 Aug 2008 21:37:16 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
content-transfer-encoding:
base64
Content-Type:
text/plain; charset="utf-8"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
1.

--------------------------

Sent using BlackBerry





----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Sun Aug 31 13:58:48 2008

Subject: Re: [TN] Question about heat transfer



Hi,





Thank you for your answers. Let me try to rephrase my question. What cooling

conditions will be more efficient, For example: if I want to reduce the PCB

temperature from 200º to 100º,

1. Air temperature is 40º and the flow is X.

or

2. Air temperature is 80º and the flow is 2X.

The flow is the amount of air flowing over the board during cooling zones.

(Not the slope….)



Thanks,

Eli.

2008/8/27, Eli Sarig <[log in to unmask]>:

>

> My question is related to the heat transfer at the cooling zones. I want to

> reduce the substrate temperature from 200º C to 100ºC; can you explain the

> relationship between the flowing air temperature and the flow rate? What

> is more important: the temperature of the air or the flow rate?

> Thanks,

> Eli.

>



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.


ATOM RSS1 RSS2