TECHNET Archives

April 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 5 Apr 2018 10:28:15 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Michels <[log in to unmask]>
Message-ID:
Subject:
From:
Bill Michels <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (32 lines)
Hello Victor,

There is no allowance for a fractured solder joint as any fracture can
further propagate during thermal cycling and cause an open circuit.

Regards,

William Michels 
CIT IPC-A-610
CIT J-STD-001


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Thursday, April 05, 2018 9:48 AM
To: [log in to unmask]
Subject: [TN] IPC-A-610G, section 5.2.9,, Solder anomalies-Fractured solder,
Defect 1, 2, 3 (Axial leaded device)

Fellow TechNetters:

   Is there a percentage associated with the statement "Fractures Solder" in
the above stated IPC STD section?
I did not a similar statement, Fractured Solder, for Surface Mount Devices
and Surface Mount Area.
Is there an acceptable percentage of the solder joint lead interface that
can be fractured?


Victor,