TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 2 Nov 2000 09:34:32 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Franklin D Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
Alloy 42 is a Nickel/Iron Alloy developed for among other reasons, it's
electrical properties in conjunction tensile/ductility. When cleaned
properly Alloy 42 should solder without any problems. One of the most
common causes of solderability failure in this alloy is the use of
non-evaporating oils during stamping/forming. Once trapped in this alloy
it is almost impossible to remove. Non-evaporating oils contain a large
amount of chlorine and sulphur both of which will wreak havoc if not
properly cleaned.

Hope this helps...

Franklin

Ron Waugh wrote:
>
>      Technetters,
>
>      I have a huge problem with the wetting and solderability of a fine
>      pitch 15 mil QFP.  I then spoke with the solder supplier; which
>      requested a couple of the components and performed x-sections.  During
>      the x-sections, they also performed a metal composition of the
>      components lead.  The metal in the leads turned out to be alloy 42,
>      which is ....non-wetting???? ...."or so I'm told".
>
>      I really don't know much about metals but the solder supplier stated
>      that the component will never wet properly.  I would really like to
>      get some literature on this alloy 42 and ask if anyone else has had
>      any of these problems and what was their fix.
>
>      Thanks in advance for your time and energy.
>
>      Regards,
>
>      Ron Waugh
>      Process Engineer
>      Diversified Systems, Inc.
>      Phone: (317) 299-9547 Ext. #336
>      Fax:  (317) 298-2055
>      Email: [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2