Florencio,
Voids in PBGA-WB components (ie. components where there is significant
decoupling between the die CTE and the substrate CTE) can be quite
forgiving. The eutectic solder balls, even with large amounts of voiding,
can have a fatigue life comparable to balls without voids.
Expect components with a higher CTE differential to the card (ie. CBGA,
etc.), to be more susceptible to void levels.
Jeff Perkins
Photocircuits
-----Original Message-----
From: Florencio Eiranova [SMTP:[log in to unmask]]
Sent: Wednesday, October 07, 1998 4:39 PM
To: [log in to unmask]
Subject: [TN] Voiding in BGA
To all:
Is there a specification to address the maximum voiding allowed
for PBGA and CBGA solder joints attached to FR-4 substrate ?
Can anybody share some personal experiences in this matter ?
Thanks
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|