TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Thu, 8 Apr 1999 09:47:35 +1000
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
Hi folks

I have this "Adverse Effect" puzzle from last CE plant ispection ; stating
we don't have validated the adverse effect of repairs ;
which unfortunately I could not argue about (this inspectors are getting
wiser every year !)

Now, before I'll scrap all the soldering irons and insist on thermal
profiles at all stages ; which is kind of radical ;
and introduce hot air jets with validated thermals ; which is kind of over
the top ;
or design it all in on p&p ; which will take time :
how do you folks address the fact we have perfectly tuned reflows and than
on the second stage we shock anything else with 0-300'C instant ? Ok ; I can
have the hotplates ; etc.; but did anybody attached thermocouples to the
manually handled component monitored throughout the process ; and
crosslinked those thermals with those specified by component manufacturer
(some caps do have very specific raise) ; flux activation recommendations ;
etc. ?
This is mainly SMD's issue ; the T/H parts with legs to dissipate the first
shock up to a degree are bit easier subject .

Thanks a lot for the help

Paul Klasek
http://www.resmed.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2