TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Foster <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 29 Jul 2014 22:59:10 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Thanks for all of the responses. There are through hole plugged vias on a very Definite grid which are very visible. They are on a 2mm grid. But other than that There are no structures in this area. The spots are very random and very hit and miss some boards 
Clean as a whistle other boards like this.
I certainly have a lot of ideas to check out now. 
I was also wondering about These black dots in the center of each of the spots. It just seems strange.
I was thinking that was the nickel plating underneath the ENIG.
This is really not my expertise so I really do appreciate all of the input 

John



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2