Immersion Silver and Immersion Tin both tarnish in the presence of Sulphides and Chlorides, and H2S and Cl are both a couple of our main target gases for our gas detection equipment. It's a black tarnish and the PCB fabricator assured us it was cosmetic only but customer perception is more important so we avoid these finishes.
James
James Head BEng CID+ MIIE MIET
Senior PCB CAD Engineer
Crowcon Detection Instruments Limited
2 Blacklands Way
Abingdon Business Park
ABINGDON
OX14 1DY
Telephone: 01235 557700 extension 289
Fax: 07092024504
E-mail: [log in to unmask]
********************************************************
The information transmitted is intended only for the person or entity to
which it is addressed and may contain confidential and/or privileged
material. If you are not the addressee, any disclosure, reproduction,
copying, distribution, or other dissemination or use of this communication is
strictly prohibited. If you have received this transmission in
error please notify the sender immediately and then delete this e-mail.
E-mail transmission cannot be guaranteed to be secure or error free as
information could be intercepted, corrupted lost, destroyed, arrive late or
incomplete, or contain viruses.
The sender therefore does not accept liability for any errors or omissions
in the contents of this message which arise as a result of e-mail
transmission. If verification is required please request a hard copy
version.
********************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|