TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Fri, 15 Oct 2004 09:40:57 +0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Le Ai Quoc <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Le Ai Quoc <[log in to unmask]>
Parts/Attachments:
text/plain (110 lines)
Thank you Ioan,
The gap between the pads is 0.3mm (if it is 0.023" (0.6mm), the chip whose
length is 0.6mm could not get good wetting in all cases). The size of pad is
0.3x0.3mm. We are using Pb-free solder paste for that PCBA. With the pad
design like this, each electrode of part will sit on pad about 0.15mm in
ideal case. How big is the misalignment which is allowed for this part?
Printing result is registered well, no offsets at placement (I checked with
microscope) and we are doing the aperture 100% as pad size.
What is the ideal time for pre-heating at reflow? Now we don't get any case
of solder ball at these chips with current profile.
I heard that there are some aperture styles which can prevent this problem.
Also, I have never heard about anti-Manhattan/tombstoning solder paste, what
is that?

Thanks and best regards,
L. A. Quoc


----- Original Message -----
From: "Tempea, Ioan" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, October 14, 2004 7:54 PM
Subject: Re: [TN] Aperture for 0603mm chip


> Quoc,
>
> I don't see you mentioning land pattern design. If the gap between the
pads
> is bigger than 0.023", you start increasing your probability of
tombstoning.
> Then, in case your soldering paste (if no-clean) does not create mid-chip
> balls, you could print 1:1, no homeplating, although we reliably do
> homeplating on 0603s that have a good pad
> design.
>
> After this you just check your process step by step: the printing shall be
> well registered, no offsets at placement and yes, the reflow recipe has an
> influence, if everything else is OK. You will need longer preheating, to
> make sure that the paste on both pads melts at the same time when hitting
> the spike. But a good reflow recipe will not correct poor printing or
> insertion.
>
> Also there are so called anti-tombstoning pastes out there, that are worth
> trying.
>
> Good luck,
> Ioan
>
> > -----Original Message-----
> > From: TechNet [SMTP:[log in to unmask]] On Behalf Of Le Ai Quoc
> > Sent: Wednesday, October 13, 2004 11:32 PM
> > To:   [log in to unmask]
> > Subject:      [TN] Aperture for 0603mm chip
> >
> > Hi Technetters,
> > Do you know the opening style (aperture) for stencil (metal mask)
applied
> > for printing solder paste on resistance, capacitor chip 0603mmm to
prevent
> > "Tombstone/Manhattan" after reflow. Also, pls. advise about stencil
> > thickness.
> > Last but not least, is the reflow profile important for this defect? Any
> > suggestion?
> > Thanks in advance,
> > Le Ai Quoc
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at [log in to unmask]
or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2