Hi Barry,
The difference between UL94 (July 29, 1997) classs are listed below.
1. Afterflame time for each individual sample t1 or t2
V-0 <=10s. ; V-1 <= 30s. ; V-2 <= 30s.
2. Total afterflame time time for any condition set (t1 plus t2
for the 5 specimens.
V-0 <=50S. ; V-1 <= 250S. ; v-2 <= 250s.
3. Afterflame or afterglow of any sample up to the holding clamp.
V-0, V-1, and V-2 Not allowed
4. Cotton indicator ignited by flaming particles or drops
V-0 and V-1 Not allowed; V-2 Allowed
Like many independent labs out there, we do this type of testing
quite a bit.
Regards,
Mike Simms
Trace Laboratories - Central
ph. 847 934 5300
fax 847 934 4600
-----Original Message-----
From: Gary McCauley [mailto:[log in to unmask]]
Sent: Thursday, October 11, 2001 10:08 AM
Subject: Re: PCB FLAME RATINGS
I believe that it is the time that it takes the material to
extinguish once the flame has been removed.
immediately vs 1 sec?
gary mccauley
-----Original Message-----
From: Barry Gallegos [mailto:[log in to unmask]]
Sent: Thursday, October 11, 2001 9:33 AM
To: [log in to unmask]
Subject: [TN] PCB FLAME RATINGS
Good morning Tech Net.
I have a question in regards to UL Flame ratings for PCB's. My incoming
inspectors have asked me what the difference is between 94V-0 and 94V-1.
any help is appreciated.
Thank you in advance.
Barry Gallegos
Process Engineer
Western Electronics
1550 South Tech Lane
Meridian, Idaho 83642
Phone: 208/955-9771
Fax: 208/955-9755
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|