TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 4 May 2006 13:44:34 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Keld Maaløe <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Keld Maaløe <[log in to unmask]>
Parts/Attachments:
text/plain (51 lines)
IPC-J-STD-020 is about Classification, I think you need IPC-J-STD-033 - "Handling, Packing, Shipping and use of Moisture/Reflow Sensitive Devices
Also avaible on JEDEC's website


Keld Maaløe
Quality Engineer
bb electronics manufacturing a/s
DK 8700 Denmark



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Daniel Blass
Sent: 3. maj 2006 21:08
To: [log in to unmask]
Subject: Re: [TN] BGA problem

Popcorning and delamination of plastic IC packages in reflow assembly is
covered by an IPC/JEDEC standard, IPC/JEDEC J-STD-020C, "Moisture/Reflow
Sensitivity Classification for Nonhermetic Solid State Surface Mount
Devices".  This standard is available free on JEDEC's website.

http://www.jedec.org/download/search/jstd020c.pdf

Daniel Blass
Process Research Engineer
Area Array Consortium
Surface Mount Technology Lab
Universal Instruments Corporation
http://www.uic.com/wcms/WCMS2.nsf/index/Global_Svc_Support_31.html

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2