Hi team - I agree with Kevin on this one. If the customer really wants a
soldered connector then they should be using a connector that is designed
for soldering. Press fit connectors are designed for interference fits and
just because they "can" be soldered, doesn't mean they should be soldered.
Many folks consider the soldering of a press fit connector a violation of
good design practices.
Dave Hillman
Rockwell Collins
[log in to unmask]
From: "Glidden, Kevin" <[log in to unmask]>
To: <[log in to unmask]>
Date: 12/03/2013 10:02 AM
Subject: Re: [TN] Press Fit
Sent by: TechNet <[log in to unmask]>
Bad idea.
For one thing, most all press-fit contacts have a hard gold finish. If
you solder this, your solder joint will be a ripe candidate for gold
embrittlement. It is a J-STD-001 requirement to remove gold prior to
soldering. And tinning prior to insertion would increase lead diameter
and insertion forces, likely leading to PTH damage.
Second, press-fit insertion is an interference fit. There was a
discussion just yesterday in TN about the criticality of getting the PCB
hole spec just right for both the drill and finish sizes. The
installation results in a hoop stress to the PTH. One can only imagine
what can happen if you then take that to solder temperatures. Lead
interference with the PTH for TH soldered applications is a no-no.
My 2 cents.
Kevin Glidden
-----Original Message-----
From: Vargas, Stephen M [mailto:[log in to unmask]]
Sent: Tuesday, December 03, 2013 10:36 AM
To: [log in to unmask]
Subject: [TN] Press Fit
All:
I have a customer who is specifying a press fit connector to be
soldered after the press fit operation. I've never heard of this and I was
wondering if there is any quality/reliability data in the industry as to
why one should/shouldn't do this. Our customer's explanation was that it
would add mechanical integrity to the joints. Thanks in advance.
Regards,
Steve Vargas
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
This E-mail is confidential. It may also be legally privileged. If you are
not the addressee you may not copy, forward, disclose or use any part of
it. If you have received this message in error, please delete it and all
copies from your system and notify the sender immediately by return
E-mail.
Internet communications cannot be guaranteed to be timely, secure, error
or virus-free. The sender does not accept liability for any errors or
omissions.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|