Graham,
You can also add the back side of leads, sharp angles, and points.
I suppose it depends on just how "lucky" you feel!
David A. Douthit
Manager
LoCan LLC
Collins Graham wrote:
> Hi Joe!
> Well, as Joyce observed, Parylene will coat everything, so that's one
> (expensive) way. Another way is to underfill the BGA before coating,
> with an underfill material. This is what we are currently doing.
>
> I do question the ability of anyone to truly meet that requirement
> though, when using a conventional spray technique. For example, if you
> have vias under components (which is pretty much standard these days)
> then you will have exposed circuitry unless you are using a dry film
> solder mask.
>
> regards,
>
> Graham Collins
> Process Engineer,
> Northrop Grumman Canada Corporation
> Halifax
> (902) 873-2000 ext 6215
>
> >>> [log in to unmask] 08/08/03 03:04PM >>>
> Tech Netters,
>
> I am looking for some input on a special issue related to the
> conformal
> coating of boards with BGAs. According to IPC-A-610C, section 9.1.2,
> voids
> in the conformal coating material can not expose circuitry, bridge
> lands or
> adjacent conductors. In order words, all exposed circuitry/conductors
> are
> to be conformally coated.
>
> BGAs have conductors/solder balls located "under" the package unlike
> leaded
> parts where the leads are exposed and easily covered with conformal
> coating
> material. Conformal coating may partially wick under the BGA covering
> some
> of the conductors/balls but not all the way. Some of the BGAs also
> stand off
> the board a measurable distance which the conformal coat material may
> not
> bridge resulting in an uncoated gap between the BGA and the pwb. Some
> would
> interpret this as leaving exposed conductors (under the BGA).
>
> I would like to know how other manufacturers are dealing with this
> issue.
> Ideally, one would seal the perimeter of the BGA with conformal coat
> thereby
> not exposing conductors but conformal coat material will not bridge
> gaps
> greater than x mils. Look forward to your response. thanks
>
> joe
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|