TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dan Brandler <[log in to unmask]>
Reply To:
Date:
Thu, 30 Oct 1997 11:41:04 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
tonghh wrote:
>
>     Hello to all technetters :
>
>     Recently I have been trying to figure out the best pretreatment method for
>     alloy42 materials for further plating processes .Could someone share some
>     info on this , since alloy42 materials is very sensitive  in nature . We
>     have tried using 5% sulphuric acid and others proprietary chemicals also
>     sulphuric acid based , the operating window is limited .
>
>     Thanks .
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
Tongh, It seems to me that 5% sulfuric is too weak. Try increasing the
concentration and/or temperature. You didn't say what is the problem
you're trying to solve, so I don't know what else to tell you. Good
luck. Dan Brandler, Technical Director, Ohmega Technology.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2