tonghh wrote:
>
> Hello to all technetters :
>
> Recently I have been trying to figure out the best pretreatment method for
> alloy42 materials for further plating processes .Could someone share some
> info on this , since alloy42 materials is very sensitive in nature . We
> have tried using 5% sulphuric acid and others proprietary chemicals also
> sulphuric acid based , the operating window is limited .
>
> Thanks .
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
Tongh, It seems to me that 5% sulfuric is too weak. Try increasing the
concentration and/or temperature. You didn't say what is the problem
you're trying to solve, so I don't know what else to tell you. Good
luck. Dan Brandler, Technical Director, Ohmega Technology.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|