TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 17 Mar 1999 15:17:39 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (108 lines)
Ha!
my past comes back to haunt me....

Well, I have been TOLD by my SUPERIORS to plate 30u over 100u nickel, and I
am telling them that that's too much gold for the SMT, but of course since
I'm "the new guy" here they need to hear it from "a reliable source" too...
(and 5u seems a little thin for contacts, I'll check into the carbon, never
tried that)

thanks everyone for the responses, I'm collating and summarizing
onward thru the fog,
Jack

                -----Original Message-----
                From:   David J. Ricketts [mailto:[log in to unmask]]
                Sent:   Wednesday, March 17, 1999 3:02 PM
                To:     'Jack Olson'
                Subject:        RE: [TN] Flash Gold and Switch Contacts

                Jack, Jack, Jack, Jack,

                All that time at the company formerly known as B/E, and you
still have gold
                questions?

                If the switch area is a contact surface, like a push button,
then consider
                screening carbon ink. Otherwise, you can flash nickel and
gold, 100 and 5
                microinches max.

                If it is a wear surface, like fingers wiping on the surface,
then you need
                electrolytic gold.

                So what kind of grass do they grow in that new valley of
yours?

                David

                MMI Designs
                voice> 949-675-7360
                fax>   949-673-3650


                -----Original Message-----
                From: TechNet [mailto:[log in to unmask]]On Behalf Of Jack
Olson
                Sent: Wednesday, March 17, 1999 9:58 AM
                To: [log in to unmask]
                Subject: [TN] Flash Gold and Switch Contacts


                I have just read through about a thousand messages regarding
gold plating in
                the Technet archive, but still couldn't find exactly what I
need to know:

                We have a design with one side all contact switch patterns,
and the other
                side SMT components. Since we wanted to gold plate the
contact patterns, we
                were told to just gold plate the whole board.

                So the question is:  What gold thickness would be thin
enough for the SMT's
                and still thick enough for good reliable contacts?  Or is
there a better
                way?

                thanks in advance,
                Jack


################################################################
                TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c

################################################################
                To subscribe/unsubscribe, send a message to [log in to unmask]
with following
                text in the body:
                To subscribe:   SUBSCRIBE TechNet <your full name>
                To unsubscribe:   SIGNOFF TechNet

################################################################
                Please visit IPC's web site (http://www.ipc.org) "On-Line
Services" section
                for additional information.
                For technical support contact Hugo Scaramuzza at
[log in to unmask] or
                847-509-9700 ext.312

################################################################


################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2