TECHNET Archives

February 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Goulet <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 11 Feb 2011 16:54:09 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (68 lines)
To Jack 

If you read you could solder to oxidized boards, the rest of the story may have referenced a certain OA flux or OA solder paste. 

The success rate of soldering to oxidized boards drops substantially when you switch to the less active No-Cleans. 

Then there is the reliability issue where it appears that the solder joint formed OK but if the board was tested in a HALT test system for stress/vibration you'd see the joint fracture way before 1000 cycles was reached. 

John Goulet 

MFG/Process Engineer 

  
----- Original Message ----- 
From: "Jack Olson" <[log in to unmask]> 
To: [log in to unmask] 
Sent: Wednesday, February 9, 2011 9:10:43 AM 
Subject: Re: [TN] IPC-4553 

Good question.... and when looking at an actual board, how is one to determine 
visually if we are looking at "staining" or "oxidation/corrosion"? Inquiring minds 
want to know. 
(many would say that even oxidized boards are solderable and acceptable. 
right? I think I just read that somewhere...) 

Jack 

. 
On Tue, 8 Feb 2011 09:20:44 -0500, Glidden, Kevin 
<[log in to unmask]> wrote: 

>Morning everyone, 
>I have a question on IPC-4553, specifically, section 3.1 "Visual", and 
specifically regarding staining of immersion silver.  The text states "The 
coverage shall be complete and the finish shall be uniform on the surface to be 
plated (see Figures 3-1 through 3-5 for properties visually identified with IAg 
plated surfaces)"  Figure 3-1 shows 'Example of Uniform Plating", with no 
staining.  Figures 3-2 through 3-5 show staining.  Is this to imply (without text 
to support) that any staining of immersion silver is determined to be non- 
uniform and therefore a defect? 
>Thanks. 
> 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2