At my previous company, we used grounded PCB racks to hold/store boards in
conjunction with the totes.  They were fully adjustable to accommodate
almost any board size and even have ESD safe covers/curtains to keep the
little gems dust free.  They can be a bit pricey but given their
adjustability, how much capacity they can hold, and the convenience of the
racks being on casters for easy mobility, it's something to consider.  We
purchased ours through Metro Carts
(http://www.intermetro.com/commercial/index.cfm).  Hope this helps.

Regards,
Mark Gilbert, Product/Process Engineer
FOX Electronics
For Frequency Control Solutions. . . Fast:
1-888-GET2FOX, ext. 2289
Direct Phone# 1-941-690-2289
Fax: 941-693-1554

http://www.foxonline.com/

 -----Original Message-----
From:   Lou Hart [mailto:[log in to unmask]]
Sent:   Friday, November 10, 2000 9:28 AM
To:     [log in to unmask]
Subject:        [TN] transporting assemblies inside manufacturing facility

TechNetters,

Please let me know of your methods for transporting assemblies in your
plants.

We have been using Olympic "totes".  These are heavy, static-shielding,
polypropylene black boxes.  But we have some assemblies that are too big to
fit inside - we can't put on the lids.  And for other reasons, we would like
to try something else.

We are looking into some containers made by Kenflex.  Their advantages are:
boxes can be custom-sized and assemblies ride is sliding, static-dissipative
polyethylene baffles.  The disadvantage is they are expensive:  depending on
number of baffles and box size, prices run in the 200$ range.  (The Olympic
totes are about 55$.)

For any comments, many thanks, muchas gracias, grazie, merci beaucoup, muito
obrigado, Danke...

Lou Hart
412-858-6184
Compunetix Quality Assurance

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2