Steve,
you might have "nice and soft gold" on day one upon receiving... but not
long...Assume you have JIT... I mean really JIT (just in hrs, may
be...hehehe) for wire bond, it would be OK...
                                jk (even in the old weather here... I
wouldn't use 20 micro-inches Ni)

abcd

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Creswick, Steven
Sent: Thursday, March 15, 2007 5:04 AM
To: [log in to unmask]
Subject: Re: [TN] IPC ENIG SPECIFICATION


Steve,

I will likely solder quite well, but the gold is quite thick for
soldering to without incurring the wrath of gold embrittlement.  I would
not be so concerned about the thin nickel as the overabundance of gold.

If the gold were nice and soft, it would be nice for gold ball bonding!
But, the nickel is quite thin.

If the numbers are correct, you did not receive ENIG - have them sent
back

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, March 14, 2007 9:31 PM
To: [log in to unmask]
Subject: [TN] IPC ENIG SPECIFICATION

Hi All,
I  have a question about this specification. Obviously when the
technical
gurus wrote this they had good reasons for specifying the nickel at a
minimum of 118 microinches. One of our customers recently received some
parts from the far east. The print called for ENIG but the parts came in
with approx. 20 microinches of nickel and approx. 40 microinches of
gold.
My question is what are the reliability/solderability concerns on low
nickel. Thanks in advance. Regards Steve Kelly

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT
FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR
THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the
intended recipient, you are hereby notified that any review, distribution,
or copying of this communication is strictly prohibited.  If you have
received this communication in error, please immediately notify the sender
by return e-mail, and delete this e-mail message and any attachments from
your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2