TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Hoover <[log in to unmask]>
Reply To:
David Hoover <[log in to unmask]>
Date:
Thu, 8 Sep 2005 20:39:45 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Is the surface finish ENIG? If so check to see if the silkscreen was applied
before the ENIG process.
I've seen this before but it was violet and /or pink.

Cheers,

David Hoover
Dir Eng and Quality
Gold Circuit Electronics GSS
San Jose, CA 95126
[log in to unmask]
www.gce.com.tw
----- Original Message -----
From: "Franklin Asbell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 08, 2005 9:38 AM
Subject: [TN] Pink symbol ink...


> We got a call from a customer expressing an interesting issue.
>
>
>
> They ran product through their wave solder and the symbolization went from
> white to pink.
>
>
>
> I've never heard of this color change appearing, anyone out there have an
> idea?
>
>
>
> The symbol is Enthone 50-100R - white, the wave solder info I have is Type
> R
> flux with a peak temperature of 215 C.
>
>
>
> Appreciate any input, thanks.
>
>
>
> Franklin
>
> pI
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Letter content was scanned by WinAntiVirus 2005.
No threat detected.
Please visit www.winantivirus.com for more details.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2