So Bev,
LF residues really are more reactive? You seem to have done some measurements.
Thanks,
Ioan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Tuesday, January 09, 2007 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning
John,
Not if they do their homework and do the proper testing to show that the
tweak in reactivity won't put them on dangerous ground. That is why
there are tests like copper mirror, halide ion, British corrosion test,
SIR and electrochemical migration.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: January 9, 2007 12:02 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning
That's what I was thinking Brian...................8-)
With the change to lead free and the various "wetting" issues a lot of
people are using a more active flux if only to make the joints "look"
more
like 63/37 and as a result are having to use cleaning systems to remove
the
flux.
Of course the ones that do not remove the flux will find out eventually
why
they should have done!!
John
John Burke
(408) 515 4992
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|