Hi Jim! Sorry, I haven't had my Diet Coke yet so both braincells aren't
fully functional! There are a number of immersion silver chemistries
available in the industry. I have experience with two - Enthone's
Alphalevel and McDermid's Sterling. Both of these chemistries passed our
internal qualification testing with the Sterling chemistry being rated
slightly higher due to process consistency. We are gearing up to test
AtoTech's immersion silver chemistry this year. Each chemistry suppler has
a recommended finish thickness. There were a couple of very good papers at
the IPC Fall meeting covering immersion silver finishes (authors - Toscano
and Milad) - I would recommend reading those for additional insight.
Dave
"Marsico, James"
<James.Marsico@DP To: [log in to unmask]
.AIL.COM> cc:
Sent by: TechNet Subject: Re: [TN] inmmersion silver
<[log in to unmask]>
10/23/2003 08:20
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Marsico, James"
OK... but what's the recommended chemistry (or what choices are there) and
what's the recommended thickness?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: [log in to unmask]
[SMTP:[log in to unmask]]
Sent: Thursday, October 23, 2003 9:17 AM
To: [log in to unmask]; [log in to unmask]
Cc: [log in to unmask]
Subject: Re: [TN] inmmersion silver
Hi Jim! The 4-14 Plating Processes subcommittee is currently
working
on
specifications for immersion silver and immersion tin. ENIG was
covered
with the publication of the IPC-4552 specification. I would
recommend you
call out the specific immersion silver chemistry, a thickness range
and a
solderability requirement on your drawing note(s) until the 4-14
committee
can complete their work. Good Luck.
Dave
"Marsico, James"
<James.Marsico@DP To:
[log in to unmask]
.AIL.COM> cc:
Sent by: TechNet Subject: [TN]
inmmersion silver
<[log in to unmask]>
10/23/2003 06:30
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Marsico, James"
Hello Technet:
What's the best way to specify immersion silver finish on a PWB?
In
accordance with what? Thickness? Anything else?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail
to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at
[log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|