TECHNET Archives

November 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roger Mack <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 6 Nov 2009 15:11:32 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (147 lines)
I would agree, they work well. Follow the PEM guidelines. We use both the 
SMT and press in styles. Problems only occur when they are not used as 
intended.
For press in, develop a keepout zone so the strain does not crack nearby 
parts. We also do a strain test on new designs to ensure and document that 
there is no issues.
For SMT style, the recommended reflow temperatures are high. If your 
design can not handle the recommended reflow temperature make sure you 
test the pushout and torque out values for yourself for the reflow profile 
used to ensure it meets your requirements.

Always cheaper in the long run to play with a test board and develop some 
DFM rules than to experiment with new parts directly on a design.



Roger Mack  P.Eng. 
Manufacturing Specialist
Parker Hannifin Electronic Controls
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB  R3T 1T4 Canada 
direct 204 453 3339 x373
[log in to unmask]
www.parker.com/ecd







"Wolfe, Robert" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
11-06-2009 14:07
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Wolfe, Robert" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] PEM (rivets) in PCB






Henry,
Back in a previous life we used them on many boards in telecommunications 
systems
both to secure keypads etc to phone boards & module boards to main boards.
They work just fine, yes it can get a little frayed around edges, but we 
have never
seen any issues in our product type related to PEMs in boards.
They work very well when installed properly with
proper hole size.
Bob



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of henry rekers
Sent: Friday, November 06, 2009 1:55 PM
To: [log in to unmask]
Subject: [TN] PEM (rivets) in PCB

Is anybody out there aware of any spec/inspection criteria/documentation 
on how to specify/design/inspect Pem type fasteners?

We have a design that may require this, but I'm not willing to commit 
until I have some more background info.  Specifically, is this a normal 
process for a board shop?  Are there any 'gotcha's'?

Thanks.


      __________________________________________________________________
Yahoo! Canada Toolbar: Search from anywhere on the web, and bookmark your 
favourite sites. Download it now
http://ca.toolbar.yahoo.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

DISCLAIMER: This e-mail may contain information that is confidential, 
privileged or otherwise protected from disclosure. If you are not an 
intended recipient of this e-mail, do not duplicate or redistribute it by 
any means. Please delete it and any attachments and notify the sender that 
you have received it in error. Unintended recipients are prohibited from 
taking action on the basis of information in this e-mail.E-mail messages 
may contain computer viruses or other defects, may not be accurately 
replicated on other systems, or may be intercepted, deleted or interfered 
with without the knowledge of the sender or the intended recipient. If you 
are not comfortable with the risks associated with e-mail messages, you 
may decide not to use e-mail to communicate with IPC. IPC reserves the 
right, to the extent and under circumstances permitted by applicable law, 
to retain, monitor and intercept e-mail messages to and from its systems.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



PLEASE NOTE: The preceding information may be confidential or
privileged. It only should be used or disseminated for the purpose
of conducting business with Parker. If you are not an intended
recipient, please notify the sender by replying to this message and
then delete the information from your system. Thank you for your
cooperation.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2