TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Thu, 21 Sep 2006 09:57:08 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
That's correct. We are gathering a lot of data to support the premise
that SAC soldering of Copper PTHs is a no-no.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Thursday, September 21, 2006 9:49 AM
To: [log in to unmask]
Subject: Re: [TN] Dissolving copper hole wall using lead free HASL?

Well, it stripped out the "cut and paste" from the pdf of Jasbir's slide
at
IPC.  Here is what he said on the slide:


During rework with SnAgCu alloy with copper from the PCB: copper
dissolves
with increasing contact time.

Experience: PTH barrel knee erosion after  20 seconds of solder pot
dwell time

Copper dissolution is a function of  original barrel/pad thickness,
solder
temperature and alloy (tin percentage),  dwell/contact time and solder
flow rate
and type of copper plating.

Studies are ongoing with dissolution rate comparison with various
lead-free
solder alloys and process optimization.


Denny Fritz

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2