Hi Technet Members,
We have been encountering several miscorrelation callouts with our
suppliers with regards to the measurement of the ENIG coating of the
PCBs we order from them. This is considering different equipment sets
used (suppliers normally use the Oxford CMI 900 while we use the
Fischerscope XDAL), and collimator sizes. All other settings are taken
from IPC 4552. I would like to clarify a few points:
1. When taking the actual thickness to be reported, should we take
readings from multiple pads and take the average? Should the average be
the reported value? In case one pad fails but the average passes, should
the board be judged as acceptable?
2. Does the IPC 6012 rev C supersede even the Amendment in IPC
6012 B which states that the requirement for gold thickness only applies
to non-solderable surfaces? Does this mean that the 0.05um minimum
thickness specified in the IPC 6012 C would apply to all pads?
Thank you,
Ann Jovelyn B. Tan
Supplier Quality Engineer
Corporate Quality and Reliability
Integrated Microelectronics, Incorporated
#103 Trade Avenue cor Technology Avenue
Special Export Processing Zone
Laguna Technopark, Phase 4 Binan, Laguna 4024
Philippines
Tel: +63 49 541 2440 to 55 local 3569/3550
Mobile: +63 923 288 1127
Email: [log in to unmask]
<mailto:[log in to unmask]>
http://www.global-imi.com <http://www.global-imi.com/>
A member of the IMI group of companies
IMI is a global vertically-integrated electronics manufacturing services
(EMS) provider well-known for its flexible expertise.
This is a virus free email...
This e-mail message and all contents are intended only for the named recipients(s). The information contained herein may be confidential or privileged, and its disclosure, distribution or reproduction is prohibited.
If you are not the named recipient, please return it immediately to its sender at the above address and destroy the original message and all copies.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|