TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bruce, David (GB - MAV)" <[log in to unmask]>
Date:
Tue, 29 Apr 2008 09:02:25 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
content-transfer-encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (124 lines)
David,
If you find software that can really do this, let us all know!

Are you thinking of Finite Element software like Ansys?  There is
another big contender also with a name starting with A, but it escapes
me right now.  If your company was a member of the CALCE consortium,
they also have truncated programs that sort of do the same thing.

The problem is:
1) The amount of computing power needed
2) Defining the problem properly
3) A lack of fundamental materials properties

Good luck!

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bruce, David (GB -
MAV)
Sent: Tuesday, April 29, 2008 4:08 AM
To: [log in to unmask]
Subject: [TN] Software package to perform fatigue life prediction of
solder joints

 

Does anyone know of a software package to perform fatigue life
prediction of solder joints.

 

I need to be able to predict the fatigue life of solder joints under
different thermal cycling and vibration load conditions. The PCB will
usually be FR4, the solder tin/lead, the components everything from
BGA's to chip passives. Ideally I need to provide an estimate on cycles
to failure.

 

We are trying to do a comparison exercise to try and specify the more
reliable component, for example, a chip capacitor in 0805 or 1206, which
one will be more reliable, from a solder joint perspective and by what
order of magnitude? And what would the expected life of the joint be
under different conditions?

 

We need to perform this exercise over a range of different types of
components, using different types of leaded solder and perhaps with
different board thicknesses. Predictive software would be quicker and
easier than empirical experiments.

 

Any ideas?

 

Regards

 

David



This email may contain proprietary information and/or copyright
material. This email is intended for the use of the addressee only.
Any unauthorized use may be unlawful. If you receive this email by
mistake, please advise the sender immediately by using the reply
facility in your email software.

Information contained in and/or attached to this document may be
subject to export control regulations of the European Community, USA,
or other countries. Each recipient of this document is responsible to
ensure that usage and/or transfer of any information contained in
this document complies with all relevant export control regulations.
If you are in any doubt about the export control restrictions that
apply to this information, please contact the sender immediately.

Be aware that Meggitt may monitor incoming and outgoing emails to
ensure compliance with the Meggitt IT User policy.

Products and services are supplied on the terms of our Standard
Selling Conditions. A copy is available on request.

Meggitt (UK) Limited trading as Meggitt Avionics
Registered Number: 629814
Registered in England and Wales
Registered Office: Atlantic House, Aviation Park West, Bournemouth
International Airport, Christchurch, Dorset BH23 6EW

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2