TECHNET Archives

July 2017

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Tue, 25 Jul 2017 19:33:42 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (33 lines)
you mean alpha particle free or low sand?
On Jul 25, 2017, at 2:12 PM, Richard Kraszewski wrote:

> Last week I heard an interesting story  NPR  radio, claiming  that  
> there is an upcoming global scarcity of sand.
>
> Seems like most  good deposits are  being mined out for concrete.   
> This is starting to  become a  concern for  people such as silicon  
> wafer producers amongst others.
>
>
>
> Anyone  hear  anything similar?
>
>
> Rich  Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp.  
> and may contain information which is privileged, confidential, and/ 
> or protected by non-disclosure agreements.  They are intended  
> solely for the use of the named addressee(s).  .  Any unauthorized  
> use or disclosure may be unlawful.  If you are not a named  
> addressee, you must not use, disclose, retain or reproduce all or  
> any part of the information contained in this e-mail or any  
> attachments If you have received this transmission in error, please  
> destroy it and notify us immediately by return e-mail or by calling  
> + 1 888 208 9005.

ATOM RSS1 RSS2