What temp are you baking the boards at and how do you rack them ?
Also why do you do UV ?
Most shops only thermal cure peelables at 150 C for 5-15 minutes
You could try curing it at 140 C .
On the UV .How many joules and what does temp do these boards see
afri
-----Original Message-----
From: S.R. Madhuchandra [mailto:[log in to unmask]]
Sent: Monday, October 20, 2003 2:12 AM
To: [log in to unmask]
Subject: [TN] Warpage after PLSM
fellow technetters
In some of the part numbers, we are facing a strange phenomenon
The boards will be flat till the process of PLSM(peelable solder mask)
but after the PLSM, there will be severe warpage & wobbling
In PLSM, we are doing both UV & thermal curing
Can some one throw some light on this
Thanks in advance
Madhu
Scan by AT&S virus protection
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|