Hey Lamar,
When we looked into this circa 2001, we learned that most or all tape brands were buying generic "tape logs" from manufacturing wholesalers. These tape log manufacturers have a trade association that publishes methods/specs. At some point, most or all of the wholesalers had moved to these specs exclusively, hence dropping support for other specs- for instance the CID-A-A-113 (the one we needed).
Recently we found that 3M is again certifying to some other specs. For instance, the 600 again lists the CID.
So try 3M. If you still have trouble, hunt up a log manufacturer that will answer the phone. The extra value is that he might be able to tell you the 18 different brands it is sold under.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lamar Young
Sent: Wednesday, September 02, 2009 11:50 AM
To: [log in to unmask]
Subject: [TN] Adhesion tape test
I need help finding a suitable replacement tape to perform adhesion testing per ASTM D3359, the tape test method.
The Permacel 99 tape that was mentioned is no longer available. We have tried a replacement tape recommended by a tape vendor, but the backing released from the adhesive during the test (the adhesive stuck better to the substrate than the backing).
Any help would be much appreciated.
Lamar
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|