Hi Joyce,
Pls see my answer to Peter.
>Re-HASL board got thicker IMC,
***Certainly true
>it fails early at end of life with high vib and high TC extreme.
***Have not seen data that show re-HASL'ed PCA failing earlier than just once
HASL'ed PCAs; the failures also are not in the IMC.
Regards,
Werner Engelmaier
---------------------------------------------------