Hi Everyone,
I have a process in our repair center that is removing a 68 pin PLCC through
hole socket with a selective soldering station. Once all of the solder
joints have become molten, a pair of needle nose pliers are used to remove
the socket from the board (pretty high tech, eh?). Does anyone know of a
better tool that could be employed? Does anyone make a tool that could grab
the socket on all four sides simultaneously?
Thank you,
Paul Black
Manufacturing Engineer
Kronos
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|