To Victor. 

Hi Victor,

I've readed your question. Please find here enclosed different alloys with
low meelting point, that my company manufactures:

67Sn 33Cd....176ºC
66,5Sn 29Cd 4,5Zn....158ºC
50Sn 32Pb 18Cd....145ºC
60Bi 40Cd....144ºC
60Sn 40Bi....138-170ºC
57Bi 43Sn....138ºC
56Bi 40Sn 4Zn....130ºC
55,5Bi 44,5Pb....124ºC
55Bi44 Pb1Sn....117-120ºC
54Bi 26Sn 20Cd....103ºC
52,5Bi 32Pb 15,5Sn....96ºC
52Bi 40Pb 8Cd....92ºC
50Bi 25Pb 12,5Sn 12,5Cd....70-72ºC
49,5Bi 27,5Pb 13Sn10Cd....70ºC

Concerning pricesor additional informatio, as Technet is a technical forum,
I preffer you will contact me by fax, or directly to my E-mail.

Best regards
                     =============
                     ANTONI CHERTA
                         (Barcelona)
                   Ph:+34.07.20.49.42
                   Fx:+34.3.274.00.80
            E-mail: [log in to unmask]
            =====================

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2